Alloy Digest (1979) 28 (3): Pt-3.
Published: 01 March 1979
... ZGS 10% Rhodium-Platinum is a grain stabilized platinum-base alloy containing a small amount of highly dispersed zirconium oxide. Its production and general characteristics are closely related to those of ZGS Platinum which also is strenghtened by highly dispersed zirconium oxide (Alloy Digest Pt...
Journal Articles
Alloy Digest (1988) 37 (3): Pt-4.
Published: 01 March 1988
... ZGS 5% RHODIUM-PLATINUM is a zirconia grain stabilized (ZGS) platinum alloy. The ZGS alloys are used to contain molten glass, one of the most corrosive materials known to man. ZGS Platinum (Alloy Digest Pt-2, May 1975) and ZGS 10% Rhodium-Platinum (Alloy Digest Pt-3, March 1979) have been covered...
Journal Articles
Alloy Digest (1975) 24 (5): Pt-2.
Published: 01 May 1975
..., drawing and extruding. Wire can be cold drawn with a reduction of 98% or more without intermediate annealing. The material can be easily formed, deep drawn, pierced, punched, spun, etc. ZGS Platinum work hardens at a rate intermediate between pure platinum and 10% rhodium-platinum; this makes ZGS platinum...