Alloy Digest (1966) 15 (1): Cu-160.
Published: 01 January 1966
... ZEPHOR BRONZE is a 5% tin-phosphor bronze possessing high tensile strength, high elastic limit, good resistance to fatigue and corrosion. It is recommended for strong, corrosion resistant diaphrams, springs, and fasteners. This datasheet provides information on composition, physical properties...