Alloy Digest (1953) 2 (1): Ni-2.
Published: 01 January 1953
... DURANICKEL, formerly known as Z-Nickel, is an age-hardenable nickel alloy having high strength and high corrosion resistance in addition to high heat resistance. It is magnetic at room temperature in all conditions. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1989) 38 (3): Zn-47.
Published: 01 March 1989
... (Zinc Die Casting Alloy) UNS Z 33522 is a zinc die casting alloy having superior castability. Composition: Ahlminum Chromium Copper MwP= Magnesium Nickel Cadmium SiliCOtl Tin Iron zinc 3.9-4.3 0.2 max. O.lOmax. 0.5 max. 0.010-0.020 0.005-0.020 0.0020 max. 0.035 max. 0.0010 max. 0.0020 max. 0.075 max...
Journal Articles
Alloy Digest (1993) 42 (1): Ni-421.
Published: 01 January 1993
...-421 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1993 %P"" P-w AkayLl@8tkl201~Z'-6161 27CanfiiSlrem.OranNJ.O7050lUSA INCONEL@ ALLOY 686 (Ni-Cr-Mo-W Corrosion Resistant Nickel-Base Alloy) INCONEL ALLOY 686 has a higher Cr + MO + W content than the current generation of corrosion-resistant...
Journal Articles
Alloy Digest (1976) 25 (4): Fe-57.
Published: 01 April 1976
... TECHALLOY D is an iron-nickel-chromium electrical-resistance alloy suitable for operating in air up to 1400-1600 F. It resists heat, oxidation and corrosion to an outstanding degree. It is used as heating elements in industrial furnaces that operate in the temperature range of 1500-1800 F with...
Journal Articles
Alloy Digest (1981) 30 (2): Ni-265.
Published: 01 February 1981
... NIKROTHAL 6 is a nickel-chromium-iron electrical-resistance alloy for use in appliances and industrial furnaces. Its maximum recommended operating temperature is 1125 C (2055 F). It is highly suitable for heating elements in domestic appliances. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1955) 4 (2): SS-26.
Published: 01 February 1955
... JESSOP G.18B is an austenitic chromium-nickel corrosion and heat resistant alloy steel, having good creep and fatigue characteristics, at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1995) 44 (9): Ni-485.
Published: 01 September 1995
... Grade ET50N is a 50 Nickel-50 Chromium type alloy developed for resistance to flue gas corrosion, particularly Bunker C oil with high sulfur and vanadium. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1959) 8 (12): SS-98.
Published: 01 December 1959
... CHROMEL-D is a special 35-20 nickel-chromium alloy developed primarily for use as heating elements in industrial furnaces designed to operate in the critical temperature range between 1500 and 1800 F. with controlled atmospheres. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1956) 5 (2): Ni-23.
Published: 01 February 1956
... HASTELLOY alloy-C is a nickel-molybdenum-chromium-iron alloy, highly resistant to strongly oxidizing acids, acid mixtures, and salts as well as chlorine and chlorine-bearing compounds, and with excellent properties as high temperatures. The strength and oxidation resistance at elevated...
Journal Articles
Alloy Digest (1970) 19 (3): Ni-151.
Published: 01 March 1970
... IN-100 is a vacuum melted and investment cast nickel-base alloy recommended for turbine blades operating at 1850-1900 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Alloy Digest (1955) 4 (4): SA-29.
Published: 01 April 1955
... AISI 3140 is a nickel-chromium alloy steel of the oil hardening type. It has good hardenability and good toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on...
Journal Articles
Alloy Digest (1989) 38 (11): Ni-376.
Published: 01 November 1989
... NICKEL VAC-901 is an iron-nickel base alloy with high strength and good oxidation resistance up to 1400 F (760 C). It is precipitation hardenable and is produced by vacuum induction melting followed by vacuum are remelting which greatly minimizes directionality of properties in large billets and...
Journal Articles
Alloy Digest (1997) 46 (7): Ni-527.
Published: 01 July 1997
... HPM beryllium-nickel alloy is capable of achieving high strength through precipitation heat treatment with excellent spring characteristics at temperatures to 550 deg F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1985) 34 (5): Ni-315.
Published: 01 May 1985
... to 13OO F (705 (Z), held at temperature for 20 hours and air cooled. Background on Welding Nickel Alloys: Different but not difficult is often the way welding of nickel alloys is described. Virtually all nickel allovs have good weldability. but they have certain characteristics that make them...
Journal Articles
Alloy Digest (1973) 22 (11): Ag-7.
Published: 01 November 1973
... Ag-Ni-Con comprises a family of silver-nickel materials ranging from 100% fine silver to 50% silver-50% nickel (by weight). These materials are used in many contact applications where they provide the desired resistance to mechanical and electrical wear and the electrical and thermal conductivity...
Journal Articles
Alloy Digest (1984) 33 (12): Ni-307.
Published: 01 December 1984
...) Diameter. in. 3 32 I.18 5!32 3.116 mm 2.4 3.2 4.0 4.8 Length. in. 9 12 I4 14 mm 229 305 356 356 Current. amperes 45-60 65-90 90- 120 130-160 :z ote: INCO-WELD B Electrode can be operated in all welding positions. Background on Welding Nickel Alloys: characteristics that make them different to weld when...
Journal Articles
Alloy Digest (1980) 29 (11): SA-378.
Published: 01 November 1980
.../asm.ad.sa0378 Copyright © ASM International® 1996 105 NORMALIZED A 203 CR. A 0 T.S. 0 Y.S J -250 -200 -150 -100 -50 0 50 100 TEMPERATURE - F Fig. 1 - Effect of temperature on tensile and yield strength of normalized 2%% nickel steel. El . m I. . . . . . c t 100. A 203 GRADE A I NORMALIZED s 80. z . z UJ 60. E...
Journal Articles
Alloy Digest (1993) 42 (6): Ni-434.
Published: 01 June 1993
... turbine discs CRUCIBLE P/M RENE 95 AND z NM34 SUPERSOLVUS RENE 95 JUNE 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS CRUCIBLE P/M RENE 95 AND SUPERSOLVUS RENE 95 (High Strength High Temperature Nickel-Base Alloy) P/M RENE 95 is a high strength, high temperature alloy used for rotating jet turbine...
Journal Articles
Alloy Digest (1967) 16 (3): Ni-122.
Published: 01 March 1967
... CHROMIC-C is a nickel-chromium-iron electrical resistance alloy recommended for use in applications where the maximum operating temperature does not exceed 1700 F (927 C). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1966) 15 (10): Cu-170.
Published: 01 October 1966
... COPEL is a copper-nickel alloy having excellent mechanical and electrical properties. It is recommended for use in electrical instruments and similar apparatus where mechanical stability and a known low coefficient of resistance are required. This datasheet provides information on composition...