Alloy Digest (1958) 7 (8): SA-74.
Published: 01 August 1958
... Yoloy-S is a nickel-copper alloy steel recommended for use where yield points higher than 50,000 psi are required, together with good formability as hot rolled and greatly increased resistance to atmospheric corrosion. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1953) 2 (1): SA-5.
Published: 01 January 1953
... Steels and two commercial steels 3 x 5 x 0.020 thick were mounted vertically in a wooden rack on a remote section of New Jersey Ocean Beach. The time elapse to the tist perforation is given below: Ingot Iron (0.04% C) 1.5 Steel (0.07% c. 0.17% Cu) 1.5 s&d (0.07% C, 0.61% CU, 1.39% Ni) over5 Std (0.11...