1-2 of 2 Search Results for

YSS YEM-K

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (3): TS-748.
Published: 01 March 2018
... Ltd Copyright ┬ę ASM International┬« 2018 2018 ASM International chemical composition heat treatability YSS YEM-K Standard grade for hot forging. YEM-K is an improved high temperature JIS-SKD7 steel. Chemical Composition, wt.% (Typical) Other special elements added, P and S...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (5): TS-749.
Published: 01 May 2018
... YSS MDC-K is a hot work tool steel grade for hot forging dies. It is a modification of JIS-SKD8 steel. This datasheet provides information on composition and hardness. It also includes information on heat treating. Filing Code: TS-749. Producer or source: Hitachi Metals America Ltd. Producer...