1-1 of 1 Search Results for

YSS DAC 55

Sort by
Journal Articles
Alloy Digest (2018) 67 (2): TS-747.
Published: 01 February 2018
... YSS DAC 55 is a standard grade for die casting dies. Tool steel for large or squeeze die casting molds with excellent heat crack resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat...