Alloy Digest (1971) 20 (4): SA-264.
Published: 01 April 1971
... YOLOY-T is a hot-rolled, fully-killed steel with a fine-grain ferritic structure and excellent forming characteristics. It is furnished at minimum yield strengths of 50,000 and 60,000, psi. This datasheet provides information on composition, physical properties, elasticity, tensile properties...
Journal Articles
Alloy Digest (1971) 20 (3): SA-261.
Published: 01 March 1971
... at room temperature. If salts are present. the corrosron rate may be increased. They are readily attacked by acids, but reasonably resistant to alkalis at ordinary temperatures. (A modified grade is available, designated Yoloy T, which has atmospheric corrosion resistance four or more times that of carbon...