Alloy Digest (2017) 66 (9): SA-800.
Published: 01 September 2017
... XABO 1300 is a liquid-quenched and tempered heavy plate product in thicknesses from 4–10 mm (0.16–0.39 in.). The US equivalent is SABO 190. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information...