Alloy Digest (2018) 67 (6): Cu-874.
Published: 01 June 2018
... Wieland K20/21 is a deoxidized copper. K21 has lower impurities than K20. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...