Alloy Digest (2007) 56 (9): Cu-751.
Published: 01 September 2007
... Wieland-BC8 is a phosphor bronze containing finely distributed lead particles. BC9 is a bronze alloy with high polishability and is often used in the jewelry industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...