Alloy Digest (2012) 61 (11): Cu-814.
Published: 01 November 2012
... Wieland-B18 Supralloy is an advanced version of B18 (Alloy Digest Cu-696, January 2003). It has a combination of useful properties, particularly for the connector spring market. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend...