Alloy Digest (2020) 69 (11): Ta-14.
Published: 01 November 2020
... Wieland Duro Tantalum is unalloyed tantalum that is produced from powder metallurgy consolidated ingots. It is a versatile refractory metal that is used in demanding applications requiring resistance to high temperature and corrosion. This datasheet provides information on composition, physical...