Alloy Digest (2020) 69 (12): Mo-20.
Published: 01 December 2020
... Wieland Duro TZM is a molybdenum-titanium-zirconium-carbon alloy produced from pressed-and-sintered billets. Compared to unalloyed molybdenum, it exhibits higher recrystallization temperature and enhanced high-temperature strength and creep strength. Wieland Duro TZM is typically used between 700...