Alloy Digest (1962) 11 (8): Cb-1.
Published: 01 August 1962
... Westinghouse Alloy B33 is a columbium-base alloy for high temperature applications requiring moderate strength where excellent fabricability, weldability, and resistance to liquid metal corrosion are prime requisites. This datasheet provides information on composition, physical properties...