Published: 01 May 2004
... Weldural is a mold alloy for applications in the low-pressure molding of rubber and other elastomers at temperatures in the 175 to 205 deg C (350 to 400 deg F) range. These applications need a mold alloy with moderate strength and good property retention at moderately elevated temperatures. Alloys...