Alloy Digest (2007) 56 (5): SA-567.
Published: 01 May 2007
... Weldox 700 is a general structural steel with a minimum yield strength of 700 MPa (102 ksi). This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA...