Alloy Digest (2007) 56 (4): TS-646.
Published: 01 April 2007
... Weartec SF is a spray formed cold-work tool steel offering a combination of high wear resistance and very good resistance to chipping, along with good toughness and ductility. Weartec SF is suitable for the production of cutting rolls and slitter knives. This datasheet provides information...