Alloy Digest (1965) 14 (10): Cu-156.
Published: 01 October 1965
... Wearite 4-13 is a corrosion and wear resistant extruded aluminum bronze preheat treated to high strength and hardness levels. It is recommended for sliding contact applications where wear resistance and non-galling characteristics are desired. This datasheet provides information on composition...