Alloy Digest (1999) 48 (10): Cu-633.
Published: 01 October 1999
... WRM alloy 5078 is a modified phosphor bronze with good electrical conductivity and improved tensile strength and stress relaxation. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. Filing Code: CU-633. Producer or source: Waterbury...