1-2 of 2 Search Results for

WRM alloy 4252

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (7): Cu-619.
Published: 01 July 1998
... WRM alloy 4252 is a modified copper-zinc-tin alloy similar to C42500 (see Alloy Digest Cu-280, June 1974), with improved conductivity, strength, and forming properties. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CU-619. Producer or...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-644.
Published: 01 January 2000
....% %IACS MPa ksi MPa ksi in 2 in., % WRM 4260 (C42600) 1 2 hard (HO2) 88.5 Cu, 8.3 Zn, 3.0 Sn, 0.10 Ni, 0.10 Fe, 0.03 P 25 496 600 72 87 448 552 65 80 12 24 WRM 4252 (C42520) 1 2 hard (HO2) 89.8 Cu, 8.0 Zn, 2.0 Sn, 0.10 Ni, 0.10 Fe, 0.03 P 30 462 565 67 82 414 517 60 75 20 min C52100 1 2 hard (HO2) 92.0 Cu...