Alloy Digest (2002) 51 (1): Cu-675.
Published: 01 January 2002
... Wieland-Z35 is a medium leaded grade with a good cold-working capacity. The alloy contains arsenic and becomes dezincification resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...