Alloy Digest (2013) 62 (12): Cu-827.
Published: 01 December 2013
... Wieland S39 has good hot working properties. The alloy also weathers well in architectural applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...