Publisher: Journals Gateway
Alloy Digest (2004) 53 (4): Cu-713.
Published: 01 April 2004
... Wieland-M30 has excellent cold working properties and good strength. The alloy is used in decorative products. It is commonly called cartridge brass, spinning brass, or extra-quality brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (3): Cu-698.
Published: 01 March 2003
..., IL 60090 (847) 537-3990 (847) 537-4085 (fax) In Germany: Wieland-Werke AG D-89070 Ulm +49-0731-944-0 +49-0731-944-2772 (fax) e-mail: info@wieland.de ISSN: 002-614X Cu-698B Table 2 Comparison of Processing Information to Other Copper Alloys M05 M10 M15 M20 M28 M30 M33 Symbol CuZn5 CuZn10 CuZn15 CuZn20...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (4): Cu-700.
Published: 01 April 2003
... (fax) In Germany: Wieland-Werke AG D-89070 Ulm Germany +49-0731-944-0 +49-0731-944-2772 (fax) e-mail: info@wieland.de ISSN: 002-614X Cu-700B Table 2 Comparison of Processing Information to Other Copper Alloys M05 M10 M15 M20 M28 M30 M33 Symbol CuZn5 CuZn10 CuZn15 CuZn20 CuZn28 CuZn30 CuZn33 Machining...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (3): Cu-711.
Published: 01 March 2004
... Wieland-M20 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn products such as lipstick cases. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (5): Cu-714.
Published: 01 May 2004
... Wieland-M33 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn decorative products and in electrical components. The alloy is often called yellow brass, 65%. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (6): Cu-716.
Published: 01 June 2004
... Wieland-M37 has excellent cold-working properties and corrosion resistance. The alloy is used in the deep-drawn and stamped condition for electrical products. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (7): Cu-718.
Published: 01 July 2004
... Wieland M36 has excellent cold-working properties. The alloy is used in decorative products, especially for mirror-polished applications. The alloy is commonly called yellow brass. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (10): Cu-690.
Published: 01 October 2002
... Wieland-M05 is copper-zinc bronze alloy with good conductivity and beautiful red color. The color allows the alloy to be used in decorative applications. The alloy has also been called gilding metal 95%, and CA 210. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (12): Cu-694.
Published: 01 December 2002
... Wieland-M15 is copper-zinc alloy with good electrical conductivity and a red color useful in decorative applications. The alloy has also been called red brass, 85%, and CA 230. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (11): Cu-692.
Published: 01 November 2002
... Wieland-M10 is a Cu-10Zn bronze alloy with good conductivity and a beautiful golden red color, making the alloy useful for decorative applications. The alloy has also been called commercial bronze, 90%, and CA 220. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (8): Cu-735.
Published: 01 August 2005
...) In Germany Wieland-Werke AG D-89070 Ulm Germany +49-0731-944-0 +49-0731-944-2772 (fax) e-mail: info@wieland.de www.wieland.com ISSN: 002-614X Cu-735B Table 2 Comparison of Processing Information to Other Copper Alloys M05 M10 M15 M20 M28 M30 M33 Symbol CuZn5 CuZn10 CuZn15 CuZn20 CuZn28 CuZn30 CuZn33...