Alloy Digest (2001) 50 (5): Cu-666.
Published: 01 May 2001
... Wieland-K75 is an improved copper alloy with uniformly dispersed precipitates for relaxation strength. The alloy is used in electro-mechanical components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...