Alloy Digest (2015) 64 (12): Cu-846.
Published: 01 December 2015
... Wieland-K15 is a deoxidized copper with low residual phosphorus. The alloy has good cold working properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance...