Alloy Digest (2011) 60 (8): Cu-801.
Published: 01 August 2011
... Wieland-FX9 is a high-manganese bronze alloy that has good strength and is available in numerous cold work tempers related to its minimum tensile strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...