Alloy Digest (2005) 54 (3): Cu-731.
Published: 01 March 2005
... Wieland-B15 is a phosphor bronze that is a widely used because it has a combination of cold-working and strength properties. It is particularly widely used in the electronic market for connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (2012) 61 (7): Cu-808.
Published: 01 July 2012
... Wieland B14 Supralloy is an advanced version of B14 (Alloy Digest Cu-686, August 2002). It has a combination of properties, particularly for the connector market. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also...