Alloy Digest (1959) 8 (5): SS-87.
Published: 01 May 1959
... WESTINGHOUSE W545 is a heat treatable iron-base alloy having good high temperature strength and oxidation resistance. It is corrosion and heat resistant. Temperature range of principal usage is 1100 F. to 1350 F. Made by Consumable Electrode Vacuum Arc Melting Only. This datasheet provides...