Journal Articles
Alloy Digest (1993) 42 (2): Ni-84.
Published: 01 February 1993
... WAUKESHA METAL NO. 88 is a corrosion resistant nickel-base alloy compounded to run against stainless steel without galling or seizing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1993) 42 (4): Ni-426.
Published: 01 April 1993
... International® 1996 Machinability: Waukesha alloy 54C machines similarly to Waukesha alloy 88 (see Alloy Digest Ni-84). For specific recom- mendations, contact the producer. General Characteristics: Waukesha alloy 54C is the highest strength alloy in the Waukesha group, has good corrosion resistance and can...
Journal Articles
Alloy Digest (1993) 42 (3): Ni-49.
Published: 01 March 1993
... WAUKESHA METAL NO. 23 is a nickel-base casting alloy having high resistance to corrosion, good machinability, and freedom from any tendency to seize or gall. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...