Alloy Digest (1979) 28 (10): TS-354.
Published: 01 October 1979
... WANDO belongs to that class of oil-hardening tool steels known as non-deforming steels. It will develop full hardness on oil quenching from a relatively low temperature with minimum volume change, hence non-deforming. It is a general-purpose tool and die steel. Among its many applications are dies...
Journal Articles
Alloy Digest (1955) 4 (9): TS-38.
Published: 01 September 1955
... (Jessop) Badger ( Latrobc) Teenax- (Simonds) Wando (Universal-Cyclops) Colonial No. 6 (Vanadium Alloys) Vulcan Oil Hardening (Vulcan) General Characteristics: UHB-46 is an oil hardening, non-deforming alloy tool steel of excellent toughness and wear resistance. It is deep hardening and will withstand many...