Alloy Digest (1995) 44 (8): Co-98.
Published: 01 August 1995
... Wallex Nos. 55 and 505 are similar composite hardfacing powders with different mesh size for different application methods. The minimum hardness is RC 58. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance...