Alloy Digest (1954) 3 (8): TS-23.
Published: 01 August 1954
... VEGA is a manganese, chromium, molybdenum alloy steel combining the deep hardening characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2020) 69 (11): TS-803.
Published: 01 November 2020
... CarTech A6, also known as CarTech Vega, is an air-hardening, high-carbon (0.70%), Mn-Cr-Mo, alloy cold-work tool steel. It combines the deep-hardening and minimum size change characteristics of air-hardening tool steels with the simplicity of low-temperature heat treatment possible in many oil...