Alloy Digest (2005) 54 (7): SA-547.
Published: 01 July 2005
... VascoMax C-200 is a cobalt-containing maraging steel with cobalt providing the primary strengthening. The number in the alloy name is representative of the ultimate tensile strength expressed in ksi. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1986) 35 (8): SA-422.
Published: 01 August 1986
... tensile strength of 212,200 psi. Table 3 - NOMINAL ROOM-TEMPERATURE PROPERTIES OF VascoMax T-200 AFTER AGING AT 900┬░F Stock TesI Tensile Yield Strength Elongation Reduction Rockwell Under Specimen Strength (0.2g Offset) (4.5 \rA) of Area C Test OrienIaIion psi Ps o/O % Hardness 9 16-m. round Longitudinal...
Journal Articles
Alloy Digest (1982) 31 (10): SA-387.
Published: 01 October 1982
... Nickel and Teledyne Vasco. International Nickel holds the patent rights. Composition: (Nominal) VascoMax VascoMax T-250 c-250** Nickel Cobalt Molybdenum Titanium Aluminum 18.50 18.50 None 7.50 3.00 4.80 I A0 0.40 0.10 0. IO *The prefvt T is for titanium-strengthened grade. **The prefix C...
Journal Articles
Alloy Digest (1990) 39 (12): SA-454.
Published: 01 December 1990
... VASCOMAX T-300 is an 18% nickel maraging steel in which titanium is the primary strengthening agent. It develops a tensile strength of about 300,000 psi with simple heat treatment. The alloy is produced by Vacuum Induction Melting/Vacuum Arc Remelting. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (5): SA-251.
Published: 01 May 1970
... VascoMax 350 CVM is an ultra-high-strength steel responding to a maraging heat treatment. It has superior notch toughness and ductility at the high yield strength level of 340,000 psi and above. It is recommended for aerospace and rocket equipment and structures. This datasheet provides...