Alloy Digest (1964) 13 (2): TS-143.
Published: 01 February 1964
... VASCO-MC is a medium carbon, chromium, molybdenum mold and cavity steel recommended for molds where good machinability and high surface finishes are desired. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...