Skip Nav Destination
Close Modal
Search Results for
Vallourec VM 80 13CR
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4
Search Results for Vallourec VM 80 13CR
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
VALLOUREC VM 80 13CR: Oil Country Tubular Goods (OCTG) Line Pipe
Available to Purchase
Alloy Digest (2016) 65 (2): CS-195.
Published: 01 February 2016
... Vallourec VM 80 13CR (minimum yield strength 80 ksi, or 550 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Abstract
View articletitled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> <span class="search-highlight">80</span> <span class="search-highlight">13CR</span>: Oil Country Tubular Goods (OCTG) Line Pipe
View
PDF
for article titled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> <span class="search-highlight">80</span> <span class="search-highlight">13CR</span>: Oil Country Tubular Goods (OCTG) Line Pipe
Vallourec VM 80 13CR (minimum yield strength 80 ksi, or 550 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: CS-195. Producer or source: Vallourec USA Corporation.
Journal Articles
VALLOUREC VM 85 13Cr: Oil Country Tubular Goods (OCTG) Line Pipe
Available to Purchase
Alloy Digest (2016) 65 (4): CS-198.
Published: 01 April 2016
... Vallourec VM 85 13Cr (minimum yield strength 85 ksi, or 586 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Abstract
View articletitled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 85 <span class="search-highlight">13Cr</span>: Oil Country Tubular Goods (OCTG) Line Pipe
View
PDF
for article titled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 85 <span class="search-highlight">13Cr</span>: Oil Country Tubular Goods (OCTG) Line Pipe
Vallourec VM 85 13Cr (minimum yield strength 85 ksi, or 586 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: CS-198. Producer or source: Vallourec USA Corporation.
Journal Articles
VALLOUREC VM 90 13CR: Oil Country Tubular Goods (OCTG) Line Pipe
Available to Purchase
Alloy Digest (2016) 65 (3): CS-197.
Published: 01 March 2016
... Vallourec VM 90 13CR (minimum yield strength 90 ksi, or 620 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Abstract
View articletitled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 90 <span class="search-highlight">13CR</span>: Oil Country Tubular Goods (OCTG) Line Pipe
View
PDF
for article titled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 90 <span class="search-highlight">13CR</span>: Oil Country Tubular Goods (OCTG) Line Pipe
Vallourec VM 90 13CR (minimum yield strength 90 ksi, or 620 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: CS-197. Producer or source: Vallourec USA Corporation.
Journal Articles
VALLOUREC VM 95 13Cr SS: Oil Country Tubular Goods (OCTG) Line Pipe
Available to Purchase
Alloy Digest (2016) 65 (7): CS-200.
Published: 01 July 2016
... Vallourec VM 95 13Cr SS (minimum yield strength 95 ksi, or 655 MPa) is a super martensitic steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Abstract
View articletitled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 95 <span class="search-highlight">13Cr</span> SS: Oil Country Tubular Goods (OCTG) Line Pipe
View
PDF
for article titled, <span class="search-highlight">VALLOUREC</span> <span class="search-highlight">VM</span> 95 <span class="search-highlight">13Cr</span> SS: Oil Country Tubular Goods (OCTG) Line Pipe
Vallourec VM 95 13Cr SS (minimum yield strength 95 ksi, or 655 MPa) is a super martensitic steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: CS-200. Producer or source: Vallourec USA Corporation.