Skip Nav Destination
Close Modal
Search Results for
VM12-SHC
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
VM12-SHC
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2017) 66 (9): SA-799.
Published: 01 September 2017
... VM12-SHC is a creep enhanced ferritic steel with moniker Fe-12Cr-1.5W-1.6Co-B. It has high strength with oxidation resistance. It was designed for power plant applications. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on high...
Abstract
View article
PDF
VM12-SHC is a creep enhanced ferritic steel with moniker Fe-12Cr-1.5W-1.6Co-B. It has high strength with oxidation resistance. It was designed for power plant applications. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-799. Producer or source: Vallourec Tubes France.