Alloy Digest (1995) 44 (2): SS-583.
Published: 01 February 1995
... VLX 562 is a high-strength austenitic-ferritic alloy with superior resistance than most 300 series stainless steels to stress-corrosion cracking. It is used in fresh water, where chlorides are present, and in high pressure applications. This datasheet provides information on composition, physical...