Alloy Digest (2020) 69 (11): Ni-764.
Published: 01 November 2020
... VDM 825 (Nicrofer 4221) is a titanium-stabilized fully austenitic Ni-Fe-Cr-Mo-Cu alloy that is designed for use in extremely corrosive environments. It is approved for pressure vessels with wall temperatures up to 450 °C (842 °F) according to VdTÜV and 538 °C (1000 °F) for Section VIII Division 1...
Journal Articles
Alloy Digest (2006) 55 (4): Ni-634.
Published: 01 April 2006
... 4320 Ti is an age-hardening Ni-Fe-Cr alloy with both good corrosion resistance and high strength to 550 °C (1020 °F). It is a modification of alloy 825 and is often used in down-hole applications of sour wells. Nicrofer is a registered trademark of ThyssenKrupp VDM GmbH. Tensile strength Yield...
Journal Articles
Alloy Digest (1995) 44 (12): Ni-494.
Published: 01 December 1995
... properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-494. Producer or source: VDM Technologies Corporation. Producer or Source: VDM Technologies Corporation Copyright © ASM International® 1996 1996 ASM...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
... of materials. Inconel and Incoloy are trademarks of the Special Metals Group of Companies. Nicrofer is a trademark of Krupp-VDM and 254SMO is a trademark of AvestaPolarit. Table 1 All-Weld Mechanical Properties, Typical Values as Welded TIG SAW + NiCr TIG + 165 °C (329 °F) Tensile strength, MPa (ksi) 780 (113...
Journal Articles
Alloy Digest (1988) 37 (7): Ni-358.
Published: 01 July 1988
... are also available. Applications: Industrial furnace components: gas turbine after burners. combustion chambers. tailpipes. Manufacturer: Verelnigte Deutsche Metallwerke AG Federal Republic of Germany In the USA: VDM Technologies Corp. Parsippany. New Jersey 07054. ...