1-15 of 15 Search Results for

VDM 625

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2020) 69 (6): Ni-760.
Published: 01 June 2020
... VDM 625 (Nicrofer 6020 hMo) is a nickel-chromium-molybdenum-niobium alloy with excellent resistance to a variety of corrosive media. In the soft annealed condition (grade 1), the alloy is used for wet corrosion applications and is approved by TÜV for pressure vessels in a temperature range from...
Journal Articles
Alloy Digest (2020) 69 (11): Ni-764.
Published: 01 November 2020
... process. Welding VDM 825 can be joined by all conventional welding pro- cesses. For welding, VDM 625 should be in the soft annealed condition, and be free from scale, grease, and markings. Comparable Grades VDM Metals VDM 825 (Nicrofer 4221) AFNOR NC21FeDU ASTM UNS N08825 DIN NiCr21Mo (2.4858) ISO...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
... RIMA 625, or 62-50, is a consumable or solid wire for tungsten inert gas (TIG), metal inert gas (MIG), and submerged arc welding (SAW). The consumable is used for matching the nickel-base alloy 625 or N06625 (see Alloy Digest Ni-121, February 1967) with typical composition Ni-20%Cr-9%Mo-3.5%Nb...
Journal Articles
Alloy Digest (2006) 55 (4): Ni-634.
Published: 01 April 2006
..., hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-634. Producer or source: VDM Technologies Corporation. Producer or Source: VDM Technologies Corporation Copyright © ASM...
Journal Articles
Alloy Digest (1997) 46 (7): SS-687.
Published: 01 July 1997
... information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-687. Producer or source: VDM Technologies Corporation. Producer or Source: VDM...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-568.
Published: 01 June 2001
... resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-568. Producer or source: Krupp VDM. Producer or Source: Krupp VDM Copyright © ASM International® 2001 2001 ASM International chemical composition corrosion-resistant alloys elasticity...
Journal Articles
Alloy Digest (2004) 53 (2): Ni-508.
Published: 01 February 2004
... resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-508. Producer or source: VDM Technologies Corporation. Originally published April 1996, revised February 2004. See also Alloy Digest SS-687, July 1997. Producer or Source: VDM Technologies Corporation Copyright © ASM...
Journal Articles
Alloy Digest (2021) 70 (3): Ni-768.
Published: 01 March 2021
...) (0.102) m 1.23 Inconel C-276 exhibits excellent resistance to corrosion by circular-mil/ft) (739) seawater, especially under crevice conditions that induce 1.0002 attack in other commonly used materials such as type 316 H/m austenitic stainless steel, Monel 400, and Inconel 625. (a) At 15.9 kA/m (200 Oe...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1325.
Published: 01 August 2020
... resistance, an over-matched filler metal such as 9% Mo Py- romet Alloy 625 is suggested. Passivation CarTech 25Ni-20Cr-6Mo may be passivated to remove finely divided particles of free iron from shop dirt or from machining with tools and coolants used for carbon steel. Passivation similar to that used for...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
..., typical, wt % Fe Mn Ni Cr Mo Cu F OES (mg/m3) 1 4 10 5 6 0.2 16 1 OES, occupational exposure standard limit Table 3 Materials to be Welded ASTM/UNS DIN Proprietary Alloy 59 and similar N06059 2.4605 (NiCr23Mo16Al) Nicrofer 5923hMo (Krupp VDM), Inconel Alloy 686 (Special Metals) + W, Hastelloy Alloy C2000...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-602.
Published: 01 February 2003
... N06059 DIN 2.4605 (NiCr23Mo16Al) Proprietary Nicrofer 5923hMo (Krupp VDM) Proprietary Inconel alloy 686 (Special Metals) + W Proprietary Hastelloy alloy C2000 (Haynes) + Cu Alloy C22 and similar ASTM/UNS N06022 ASTM/UNS A494 Grade CX2MW (cast) DIN 2.4602 (NiCr21Mo14W) DIN 2.4811, 2.4836 (NiCr20Mo15) DIN...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1056.
Published: 01 March 2010
... (PAW). Overmatching composition welding products such as Inconel filler metals 625 and 622 and Incoweld 686CPT and Inconel 112 and 122 and Incoweld 686CPT welding electrodes are recommended for joining alloy 25-6HN. DOI: 10.31399/asm.ad.ss1056 Corrosion Resistance: Incoloy alloy 25-6HN offers...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
.... Hastelloy and C-22 are trademarks of Haynes International, Inc. Nicrofer is a trademark of Thyssen Krupp VDM. Table 1 Typical Room Temperature Mechanical Properties of Inconel Alloy 22 Material thickness Tensile Yield strength, or diameter strength 0.2% offset Elongation, Hardness, Form mm in. MPa ksi MPa...
Journal Articles
Alloy Digest (1982) 31 (3): SS-403.
Published: 01 March 1982
... techniques and remedies. Any craters and cracks should be completely removed by grinding. INCONEL@ alloy 625 or HASTELLOY@ alloy G are recom- mended as fiuer metal. Suitable electrodes and welding wire can be obtained from various manufacturers. Dependent on the com- ponent, plate thickness, and application...
Journal Articles
Alloy Digest (1985) 34 (3): SS-458.
Published: 01 March 1985
...): approx. 2% Temperature: 20-4oOC (70-100 F) Specification Equivalents: DIN Material No. 1.4539. UNS No. NO8904 ASTM B 625. General Characteristics: Cronifer 1925LC is a low-carbon austenitic chromium-nickel stainless steel to which molybdenum (nominally 4.75%) and copper (nominal I .5%) have been added...