Skip Nav Destination
Close Modal
Search Results for
VASCO M-2
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 26 Search Results for
VASCO M-2
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1959) 8 (6): TS-7.
Published: 01 June 1959
... VASCO M-2 is a general purpose high-speed steel of the tungsten-molybdenum type. The steel combines to an excellent degree resistance to wear toughness. Not particularly susceptible to decarburization. This datasheet provides information on composition, hardness, tensile properties, and bend...
Abstract
View article
PDF
VASCO M-2 is a general purpose high-speed steel of the tungsten-molybdenum type. The steel combines to an excellent degree resistance to wear toughness. Not particularly susceptible to decarburization. This datasheet provides information on composition, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-7. Producer or source: Vanadium Alloys Steel Company. Originally published June 1953, revised June 1959.
Journal Articles
Alloy Digest (1974) 23 (11): TS-278.
Published: 01 November 1974
... VASCO M-50 is a hardenable (martensitic), low-alloy high-speed steel developed primarily for high-strength, high-load components (such as bearings and gears) designed for elevated-temperature service. It may be used at temperatures up to 600 F; this is in contrast to AISI 52100 steel which may...
Abstract
View article
PDF
VASCO M-50 is a hardenable (martensitic), low-alloy high-speed steel developed primarily for high-strength, high-load components (such as bearings and gears) designed for elevated-temperature service. It may be used at temperatures up to 600 F; this is in contrast to AISI 52100 steel which may be used up to only 350 F. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-278. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1983) 32 (11): TS-418.
Published: 01 November 1983
... applications. A second temper is mandatory and sometimes a third temper is recommended. The holding time at the tempering temperature should be about 2 hours per inch of greatest cross section. Distortion: Vasco M-30 has medium distortion when hardened by quenching in oil and low distortion when hardened...
Abstract
View article
PDF
VASCO M-30 is a high-speed tool steel containing nominally 8.70% molybdenum and 4.75% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and super-alloys. It is recommended for cutting tools requiring a good combination of suitable toughness with optimum cutting qualities. Typical applications of VASCO M-30 comprise milling cutters, broaches, drills, hobs, turning tools and dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-418. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1983) 32 (3): TS-413.
Published: 01 March 1983
... time at the tempering temperature should be about 2 hours per inch of greatest cross section. Distortion: Vasco M-33 has medium distortion when hardened by quenching in oil and low distortion when hardened by cooling in air or a molten salt bath. It has medium safety (against cracking) in hardening...
Abstract
View article
PDF
VASCO M-33 is a high-molybdenum high-speed steel containing 8% cobalt which contributes materially to the superior red hardness of the steel. It is recommended highly for tools that require the optimum combination of high-temperature hardness, resistance to wear and cutting edge strength and retention. Typical applications for VASCO M-33 include broaches, end mills, lathe tools and drills. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-413. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1981) 30 (3): TS-379.
Published: 01 March 1981
... VASCO M-7 is a molybdenum type of high-speed steel having tungsten, chromium and molybdenum contents similar to AISI Type MI high-speed steel, but with higher carbon and vanadium. The increased percentages of carbon and vanadium add to the cutting efficiency of the steel without materially...
Abstract
View article
PDF
VASCO M-7 is a molybdenum type of high-speed steel having tungsten, chromium and molybdenum contents similar to AISI Type MI high-speed steel, but with higher carbon and vanadium. The increased percentages of carbon and vanadium add to the cutting efficiency of the steel without materially lessening the toughness. This steel has met with considerable favor among high-speed steel users who are seeking improved cutting properties for specific applications. Its many applications include drills, end mills, milling cutters, punches and shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-379. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1965) 14 (1): TS-158.
Published: 01 January 1965
... joinability machinability Rockwell C70 hardness Vasco Hypercut workability Filing Code: TS-158 VASCO HYPERCUT Tool Steel JANUARY 1965 -DATA ON WORLD WIDE METALS AND ALLOYS Prblirbdby . . gn&WrmgAll~DilcEt.IllC. Upper Moatdsir, Ncr Jarcr VASCO HYPERCUT (Super-Hard High Speed Steel, Type M-42) Vasco...
Abstract
View article
PDF
Vasco Hypercut is a super-hard high-speed steel that hardens to Rockwell C70 and is recommended for cutting tools for the toughest machining operations. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-158. Producer or source: Vanadium Alloys Steel Company.
Journal Articles
Alloy Digest (1990) 39 (11): SS-516.
Published: 01 November 1990
.... The steel is produced by high quality vacuum melting. VASCO is a registered trademark of Teledyne Vasco. Composition (Nominal): Nickel Chromium Titanium Aluminum Carbon Silicon Manganese Physical Constants: 10.50 Density, lb/cu in. 12.00 Specific gravity 0.30 1.20 Thermal coef. expansion/ F (70-7WF) K (2 I...
Abstract
View article
PDF
VASCO 734 is a precipitation hardening stainless maraging steel. Its corrosion resistance in marine atmosphere is comparable to that of AISI Type 430 ferritic stainless steel. Its low predictable shrinkage reduces post-age machining and eliminates rejected parts due to warpage in heat treatment. The steel is produced by high quality vacuum melting. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-516. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1984) 33 (9): TS-428.
Published: 01 September 1984
... temperature should be about 2.5-3 hours per inch of greatest cross section. DOI: 10.31399/asm.ad.ts0428 Copyright © ASM International® 1996 Fig. 2-Cutting speed versus tool life for TeleCut and Al81 M-42 high-speed steels. equivalent to AISI Type M42 in wear resistance and surpasses it in toughness...
Abstract
View article
PDF
VASCO TeleCut is a cobalt-free high-speed steel that is a cost-effective alternative to many cobalt high-speed steels because of its special combination of hot hardness, wear resistance and toughness. TeleCut is a superior high-speed steel that is ideal for a variety of cutting tools, including end mills, milling cutters, broaches and gear cutters. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-428. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1979) 28 (7): TS-351.
Published: 01 July 1979
... lathe tools machinability physical properties VASCO 8-N-2 workability IIASCO 8-W-2 Filing Code: TS-351 Tool Steel JULY 1979 - DATA ON WORLD WIDE METALS AND ALLOYS wzz- lm Upper M-. New J~my VASCO 8-N-2* (High-Speed Steel; AISI Type Ml) VAX0 8-N-2 is a molybdenum high-speed steel containing a low...
Abstract
View article
PDF
VASCO 8-N-2 is a molybdenum high-speed steel containing a low percentage of tungsten. It can be used successfully for a variety of cutting tools; in fact, it is a general-purpose high-speed steel. Its composition represents the first molybdenum high-speed steel to be manufactured and find practical use in the field of cutting tools. Its many uses include drills, milling cutters, lathe tools, blanking dies and special shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-351. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1961) 10 (12): TS-30.
Published: 01 December 1961
... Code: TS-30 08 VASCO SUPREME-A uxmm i;lz FERRUARY 19SS DIGESTfl - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbd by VASCO SUPREME* A High gpoed Steel Type M-15 VASCO SWREME A is a new type of super-high Speed Steel possessing performance qualities far surpassing the stand- ard grades of high speed steel...
Abstract
View article
PDF
VASCO SUPREME A is a super high-speed steel possessing performance qualities far surpassing the standard grades of high-speed steel. This datasheet provides information on composition and hardness. It also includes information on forming and heat treating. Filing Code: TS-30. Producer or source: Vanadium Alloys Steel Company. Originally published February 1955, revised December 1961.
Journal Articles
Alloy Digest (1997) 46 (12): SA-491.
Published: 01 December 1997
... quench. Vasco 9430 can also be oil quenched Tempering. Vasco 9430 is tempered at 204 or 538 C (400 or 1000 OF). Double tempering for 2 h each cycle is recommended Weldability: Vasco 9430 can be welded in the annealed condition or the quenched and tempered condition. Welding is done without pte- heat...
Abstract
View article
PDF
Vasco 9-4-30 (0.30 wt% C) is a premium quality aircraft steel which combines high tensile strength with good fracture toughness. It is a heat treatable alloy capable of developing ultimate tensile strengths greater than 250 ksi. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: SA-491. Producer or source: Vasco, An Allegheny Teledyne Company.
Journal Articles
Alloy Digest (1966) 15 (8): SA-200.
Published: 01 August 1966
... iij x 325 Vasco M\trix II - CVM Aust. 15 min. Salt Quench Tempered 2+2+2 hrs. - 2025 F -- o-- 2050°F L I I I I 54 56 58 60 62 64 Rockwell C Hardness Heat Treatment Annealing: Heat to 1600-1650oF, hold ar temperature until heat is equalized, cool slowly in the furnace at a race less than 50oF/hour...
Abstract
View article
PDF
VASCO MATRIX II-CVM is a highly alloyed steel having good high temperature strength and heat resistance. It has the composition and strength of the high-speed tool-steel matrix without the embrittling carbides being present. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-200. Producer or source: Vanadium Alloys Steel Company.
Journal Articles
Alloy Digest (1984) 33 (11): TS-431.
Published: 01 November 1984
... and M IO. VascoDyr is reccmmended as an excellent alternate to the traditional high-speed steels used in cutting-tool applications. *VascoDyne is a registered trademark of Teledyne Vasco. A patent is pending on VascoDyne. Composition: Carbon 1.00 Manganese 0.25 Phosphorus 0.03 max. Sulfur 0.03 max...
Abstract
View article
PDF
VascoDyne is a high-speed steel for the metal-cutting industry. This steel is designed to give equivalent or better performance than many grades of high-speed steel now in use and at a lower cost. VascoDyne provides improved hot hardness and wear resistance over conventional high-speed steels such as AISI Types, M1, M7 and M10. VascoDyne is recommended as an excellent alternate to the traditional high-speed steels used in cutting-tool applications. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-431. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1963) 12 (1): TS-128.
Published: 01 January 1963
... VASCO VANADIUM TYPE BB is a high carbon, chromium-vanadium alloy steel of the water-hardening or oil-hardening type having high wear resistance combined with toughness. It has good depth hardenability for a water-hardening steel. This datasheet provides information on composition, physical...
Abstract
View article
PDF
VASCO VANADIUM TYPE BB is a high carbon, chromium-vanadium alloy steel of the water-hardening or oil-hardening type having high wear resistance combined with toughness. It has good depth hardenability for a water-hardening steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-128. Producer or source: Vanadium Alloys Steel Corporation.
Journal Articles
Alloy Digest (1960) 9 (7): TS-95.
Published: 01 July 1960
... VASCO CHOICE No. 1 is a 4% chromium high-carbon hot work steel especially adapted for those operations where the hot work is performed by a compressive action. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on forming...
Abstract
View article
PDF
VASCO CHOICE No. 1 is a 4% chromium high-carbon hot work steel especially adapted for those operations where the hot work is performed by a compressive action. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-95. Producer or source: Vanadium Alloys Steel Corporation.
Journal Articles
Alloy Digest (1979) 28 (10): TS-355.
Published: 01 October 1979
... as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-355. Producer or source: Teledyne Vasco. Producer or Source: Teledyne Vasco Copyright © ASM International® 1996 1996 ASM International chemical composition compressive strength cutting...
Abstract
View article
PDF
RED CUT SUPERIOR is a high-speed steel of the 18% tungsten-4% chromium-1% vanadium type. Many consider it to be the best type of high-speed steel for general purposes. It is comparatively easy to fabricate and simple to heat treat. It has a minimum tendency to decarburize and an excellent combination of cutting ability and toughness. Its many uses include drills, reamers, milling cutters, lathe tools, punches, dies and springs for use at elevated temperature. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-355. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1970) 19 (5): SA-251.
Published: 01 May 1970
...-251. Producer or source: Teledyne Vasco. Producer or Source: Teledyne Vasco Copyright © ASM International® 1996 1996 ASM International aerospace equipment chemical composition compressive strength corrosion-resistant alloys ductility elasticity fracture toughness hardness heat...
Abstract
View article
PDF
VascoMax 350 CVM is an ultra-high-strength steel responding to a maraging heat treatment. It has superior notch toughness and ductility at the high yield strength level of 340,000 psi and above. It is recommended for aerospace and rocket equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-251. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1986) 35 (8): SA-422.
Published: 01 August 1986
... 213300 207700 13.0 69.0 43.9 2 I 2-m. round Longitudinal 211600 205900 13.1 68.3 44.3 &in. square LongiIudinal 213800 208400 13.7 69.8 45.5 6-in. square Transverse 214700 209000 12.3 62.0 45.3 0.155-in. sheet Transverse 211000 205400 8.0 62.2 44.2 0.300-in. sheet Transverse 2 I2700 206100 9.0 66.7 46.2...
Abstract
View article
PDF
VascoMax T-200 is an 18% nickel maraging steel with titanium as the primary strengthening agent and containing no cobalt. It is double vacuum melted to assure high purity which is essential for optimum mechanical properties. Price stability is an advantage with titanium-strengthened maraging steels, as compared with the price fluctuations that can occur with the cobalt-strengthened steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-422. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1990) 39 (12): SA-454.
Published: 01 December 1990
... on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-454. Producer or source: Teledyne Vasco. Producer or Source...
Abstract
View article
PDF
VASCOMAX T-300 is an 18% nickel maraging steel in which titanium is the primary strengthening agent. It develops a tensile strength of about 300,000 psi with simple heat treatment. The alloy is produced by Vacuum Induction Melting/Vacuum Arc Remelting. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-454. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1969) 18 (8): TS-222.
Published: 01 August 1969
..., and elasticity as well as fracture toughness, and deformation. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-222. Producer or source: Teledyne Vasco. Producer or Source: Teledyne Vasco Copyright © ASM International® 1996 1996 ASM International...
Abstract
View article
PDF
VAN LOM is a molybdenum type high-speed steel having excellent wear and cutting properties. It is recommended for cutting tools, punches, shear blades, blanking dies, etc. where improved toughness is desired. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness, and deformation. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-222. Producer or source: Teledyne Vasco.