Alloy Digest (1997) 46 (12): SA-491.
Published: 01 December 1997
... Vasco 9-4-30 (0.30 wt% C) is a premium quality aircraft steel which combines high tensile strength with good fracture toughness. It is a heat treatable alloy capable of developing ultimate tensile strengths greater than 250 ksi. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (11): TS-418.
Published: 01 November 1983
... to annealing. Joinabllity: The weldability of Vasco M-30 tool steel is poor, but possible if carefully preheated and postheated. It can be brazed successfully with standard practices. Specification Equivalents: Al.9 M30. SAE M30. UNS No. TI 1330. General Characteristics: Vasco M-30 is a molybdenum type of high...
Journal Articles
Alloy Digest (1997) 46 (10): SA-489.
Published: 01 October 1997
... TEMPERATURE - OF Fig.2 E&x of tempering temperature. on tensile pruperties of Vasco-9- 4-20. All specimens austenitized for 30 minutes at 1550 F. water quenched, and double tempered. 2 h each time at rempemmre. vasco An Allegheny Teledyne Company Monroe, NC 28 11 l-5030 (704) 289-4511 (704) 2894018 (fax...
Journal Articles
Alloy Digest (1974) 23 (9): TS-274.
Published: 01 September 1974
...-270 l/16 l/32 45-52 190-220 118 l/32 3844 170-190 l/4 l/32 30-36 140-l 60 Workability: Vasco Tuf can be hot worked readily. Preheat and soak at 1450.1550oF, then raise the temperature slowly to 21000F. Hot work in the range 1900.21000F. Weldability: Although welding is not normally done on Vasco Tuf...
Journal Articles
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
... toughness of Va6co Wear and seven othertoolsmdr. loot Hardness - 60 Rc High value means high wear resistance 80 -Vasco 80 40 20 0 Fig. 4 - Relative war resistam of Vasco Wear and seven othertoolstds. Heat Treatment: Normalizing: Do not normalize. Annealing: Heat to 1550-1600oF, soak to equalize temperature...
Journal Articles
Alloy Digest (1979) 28 (7): TS-351.
Published: 01 July 1979
... - , , , . . . . . . lzod impact (smooth, no notch) vs. hardnetss of 9-N-2. Austanitized at 2175 and 2225oF. then quenched in oil. All specimens double tampared above 9WF to produce the-hardness indicated. b \ 2225 F F, we -0 \ \ 30 I I I I I I I I I I AI J 54 55 56 57 54 59 60 61 62 63 64 65 66 67 Hardness Rockwell C...
Journal Articles
Alloy Digest (1990) 39 (12): SA-454.
Published: 01 December 1990
... on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-454. Producer or source: Teledyne Vasco. Producer or Source...
Journal Articles
Alloy Digest (1966) 15 (12): TS-186.
Published: 01 December 1966
... as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-186. Producer or source: Teledyne Vasco. Producer or Source: Teledyne Vasco Copyright ┬ę ASM International┬« 1996 1996 ASM International chemical composition...
Journal Articles
Alloy Digest (1961) 10 (1): SA-109.
Published: 01 January 1961
... Center 325000 260000 Tempered at IOOOoF. to 300,000 Tensile: Surface 301000 248000 Mid-radius 300000 250000 Center 301000 248000 Elongation Reduction in 4D of Area % 75 4-t 416 5:9 13.1 10.4 9.3 28.8 23.2 19.6 7.75 0.280 6.1 7.1 7.4 199 199 :; 16 Charpy Impact V-notch ft. lbs. 14 I8 21 :: DOI: 10.31399...
Journal Articles
Alloy Digest (1971) 20 (1): TS-232.
Published: 01 January 1971
... are recommended for AISI Type L6: Depth Cutting speeds, sfpm, for of cut Feeds, in. per revolution, of in. l/64 l/32 1116 3132 -- High Speed Steel l/32 60-65 - 34-40 28-34 l/16 S&58 - 30-36 26-32 1/ 3 4248 - 28-34 21-26 l/4 32-38 - 22-26 16-20 l/2 22-28 - 15-22 10-15 Cast Nonferrous l/32 95-105 - 66-75 5565 l/16...