1-11 of 11 Search Results for

VANADIS 6

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2006) 55 (11): TS-637.
Published: 01 November 2006
... Vanadis 6 is a high powder metallurgy cold-work tool steel offering a combination of very high wear resistance and good toughness. It is used for long stamping runs of working materials that tend to cause mixed adhesive and abrasive tool wear. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1999) 48 (1): TS-566.
Published: 01 January 1999
...-Serv@po.ASM-Intl.org VANADIS 30 Filing Code: TS-566 Tool Steel January 1999 Table 1 Physical Properties Hardened and tempered Thermal Soft annealed Coefficient of conductivity Specific Temperature Density thermal expansion W/m Btu/ heat capacity °C °F kg/m3 (lb/in.3) 10 6/K (10 6/°F) K (h ft °F) J...
Journal Articles
Alloy Digest (2021) 70 (11): TS-820.
Published: 01 November 2021
..., p 6. For cutting data recommendations consult Uddeholm Vanadis 23 SuperClean, Uddeholms AB, 2019, p 9 10. Quenching Media. (a) Vacuum (high speed gas at sufficient overpressure, Comparable Grades Uddeholm Vanadis 23 SuperClean minimum 2 5 bar, or 29 73 psi). (b) Martempering Assab PM 23 SuperClean...
Journal Articles
Alloy Digest (2022) 71 (1): TS-823.
Published: 01 January 2022
...%(a) 2.3 (b) (b) (b) (b) 4.2 7.0 10.5 6.5 6.5 bal (a) Typical analysis. (b) Not disclosed in Uddeholm Vanadis 60 SuperClean, Uddeholms AB, 2019 Physical Properties Property Density(a) Coefficient of linear thermal expansion(b) Unit kg/m3 (lb/in.3) 10 6/K (10 6/°F) Thermal W/(m K) conductivity(b) (Btu/(h·ft...
Journal Articles
Alloy Digest (2006) 55 (5): TS-631.
Published: 01 May 2006
... Vanadis 4 Extra is a high-alloyed powder metallurgical (PM) tool steel suitable for long-run tooling in applications with high demands on adhesive wear and chipping resistance. Due to the very carefully balanced alloying and the powder metallurgical manufacturing route, Vanadis 4 Extra has better...
Journal Articles
Alloy Digest (1995) 44 (3): TS-536.
Published: 01 March 1995
... VANADIS 10 is a chromium-molybdenum-vanadium powder metallurgical cold work tool steel offering a combination of extremely high wear resistance and good toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness...
Journal Articles
Alloy Digest (2020) 69 (11): TS-804.
Published: 01 November 2020
... Uddeholm Vanadis 8 SuperClean is a high-carbon, Cr-Mo-V, alloy cold work tool steel that is produced by the powder metallurgy process. It is suitable for very long run tooling where a combination of very high wear resistance and good chipping resistance is required. This datasheet provides...
Journal Articles
Alloy Digest (1991) 40 (10): TS-506.
Published: 01 October 1991
... VANADIS 4 is a high performance cold work tool steel made by powder metallurgy. It offers an extremely good combination of resistance and toughness for high performance tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and bend strength as well...
Journal Articles
Alloy Digest (2001) 50 (12): Ti-123.
Published: 01 December 2001
... alpha-beta alloy for surgical implants. The alloy was developed specifically for the manufac- ture of femoral component items for hip prostheses. The metal- lurgy of the alloy is closely analogous to that of TIMETAL 6-4, but biocompatibility is improved with the replacement of vanadi- um by niobium...
Journal Articles
Alloy Digest (2010) 59 (3): TS-687.
Published: 01 March 2010
... Properties: Temperature °C (°F) 20 (68) 200 (390) 400 (750) Density, kg/m3 (lb/in.3) 7700 (0.280) Coefficient of thermal expansion, 20 °C (68 °F), 10 6/K (10 6/°F) 11.1 (6.1) 11.9 (6.6) Thermal conductivity(a), W/m · K (Btu · in./ft2 · h · °F) 21 ± 2 (145 ± 0.5) 25 ± 0.5 (173 ± 3) Specific heat capacity, J...
Journal Articles
Alloy Digest (1961) 10 (12): TS-70.
Published: 01 December 1961
... MAY 19s8 NOfhll 0.40 iii: 4i5 4.25 2.20 z Reminder 0.38 - 0.43 0.20 - 0.40 0.20 - 0.35 4.00-4.50 4.00-4.50 2.00 - 220 0.30 - 0.50 4.00 - 4.50 PROPERTIES 49.5 52.0 x z % 2: 31.0 99 56.5 52:s E 2150 57.0 53.5 39:s 2200 Y 59.0 55.0 i%i El iE 56.5 it! 57.0 2350 62.0 67 61:s 57.5 51.5 6% Best range for oil...