... VAN QN (80) is a dual-phase steel with an equivalent yield strength of 80,000 psi and an exceptional combination of strength, formability, weldability, toughness and fatigue resistance. A dual-phase steel is one whose microstructure primarily consists of a mixture of ferrite and martensite...