Published: 01 March 2016
... Vallourec VM 90 13CR (minimum yield strength 90 ksi, or 620 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2016) 65 (2): CS-195.
Published: 01 February 2016
... Vallourec VM 80 13CR (minimum yield strength 80 ksi, or 550 MPa) is a low alloy carbon steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...