Skip Nav Destination
Close Modal
Search Results for
Uranus 76N
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Uranus 76N
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2009) 58 (1): SS-1028.
Published: 01 January 2009
... URANUS 76N contains high chromium, molybdenum, and nitrogen contents and has a pitting resistance equivalent number (PREN) ≥ 40. These factors explain why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore applications...
Abstract
View article
PDF
URANUS 76N contains high chromium, molybdenum, and nitrogen contents and has a pitting resistance equivalent number (PREN) ≥ 40. These factors explain why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore applications. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1028. Producer or source: Industeel USA, LLC.