Skip Nav Destination
Close Modal
Search Results for
Uranus 31
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-8 of 8 Search Results for
Uranus 31
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2014) 63 (11): SS-1191.
Published: 01 November 2014
... Uranus 31 is a super-austenitic steel with very high nickel, chromium, and molybdenum content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance...
Abstract
View article
PDF
Uranus 31 is a super-austenitic steel with very high nickel, chromium, and molybdenum content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1191. Producer or source: Industeel USA, LLC.
Journal Articles
Alloy Digest (1995) 44 (8): SS-605.
Published: 01 August 1995
... URANUS B28 is an iron-31 nickel-27 chromium-3.5 molybdenum alloy for corrosion conditions, including mineral acids, even when they are contaminated with chlorides and fluorides. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear...
Abstract
View article
PDF
URANUS B28 is an iron-31 nickel-27 chromium-3.5 molybdenum alloy for corrosion conditions, including mineral acids, even when they are contaminated with chlorides and fluorides. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: SS-605. Producer or source: Creusot-Marrel.
Journal Articles
Alloy Digest (2016) 65 (10): SS-1253.
Published: 01 October 2016
... Uranus B64 is a nonmagnetic high strength stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance, corrosion resistance...
Abstract
View article
PDF
Uranus B64 is a nonmagnetic high strength stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance, corrosion resistance, and surface qualities as well as forming, heat treating, and joining. Filing Code: SS-1253. Producer or source: Industeel USA, LLC. See also Alloy Digest SS-1218, July 2015.
Journal Articles
Alloy Digest (2014) 63 (10): SS-1187.
Published: 01 October 2014
... Uranus 28 is a super-austenitic steel with very high nickel and chromium contents. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well...
Abstract
View article
PDF
Uranus 28 is a super-austenitic steel with very high nickel and chromium contents. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1187. Producer or source: Industeel USA, LLC.
Journal Articles
Alloy Digest (2015) 64 (7): SS-1218.
Published: 01 July 2015
... Uranus B64 is a pitting resistant, high-strength nonmagnetic stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance...
Abstract
View article
PDF
Uranus B64 is a pitting resistant, high-strength nonmagnetic stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: SS-1218. Producer or source: Industeel USA, LLC. See also Alloy Digest SS-1253, October 2016.
Journal Articles
Alloy Digest (2012) 61 (7): SS-1124.
Published: 01 July 2012
... Uranus 4565 is a high N super austenitic stainless steel with a Pitting Resistance Equivalent Number (PREN) >45. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes...
Abstract
View article
PDF
Uranus 4565 is a high N super austenitic stainless steel with a Pitting Resistance Equivalent Number (PREN) >45. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1124. Producer or source: Industeel USA, LLC.
Journal Articles
Alloy Digest (1999) 48 (7): SS-751.
Published: 01 July 1999
... URANUS S1 is the development of 15 years research into alloys containing high silicon contents (4% here) to resist the transpassive intergranular corrosion from such chemicals as concentrated nitric acid. This datasheet provides information on composition, physical properties, elasticity, tensile...
Abstract
View article
PDF
URANUS S1 is the development of 15 years research into alloys containing high silicon contents (4% here) to resist the transpassive intergranular corrosion from such chemicals as concentrated nitric acid. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-751. Producer or source: Cruesot-Marrel.
Journal Articles
Alloy Digest (1999) 48 (7): SS-747.
Published: 01 July 1999
... URANUS B6N is a multipurpose austenitic stainless steel with excellent corrosion properties. This alloy, developed more than 40 years ago, has been improved by the higher addition of nitrogen to approx. 0.13% to increase its structure stability and corrosion resistance. See also URANUS B66, Alloy...
Abstract
View article
PDF
URANUS B6N is a multipurpose austenitic stainless steel with excellent corrosion properties. This alloy, developed more than 40 years ago, has been improved by the higher addition of nitrogen to approx. 0.13% to increase its structure stability and corrosion resistance. See also URANUS B66, Alloy Digest SS-602, July 1995. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: SS-747. Producer or source: Creusot-Marrel. Originally published June 1999, corrected July 1999.