1-18 of 18 Search Results for

Uranus 28

Sort by
Journal Articles
Alloy Digest (2014) 63 (10): SS-1187.
Published: 01 October 2014
... Uranus 28 is a super-austenitic steel with very high nickel and chromium contents. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1999) 48 (7): SS-751.
Published: 01 July 1999
... URANUS S1 is the development of 15 years research into alloys containing high silicon contents (4% here) to resist the transpassive intergranular corrosion from such chemicals as concentrated nitric acid. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1995) 44 (9): SS-610.
Published: 01 September 1995
... URANUS B26 is a superaustenitic alloy with 6 molybdenum and a pitting resistance equivalent number (PREN) equal or greater than 43. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2014) 63 (12): SS-1194.
Published: 01 December 2014
... Uranus 926 is a super-austenitic steel with very high nickel, molybdenum, and chromium contents. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (2015) 64 (7): SS-1218.
Published: 01 July 2015
... Uranus B64 is a pitting resistant, high-strength nonmagnetic stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance...
Journal Articles
Alloy Digest (2016) 65 (10): SS-1253.
Published: 01 October 2016
... Uranus B64 is a nonmagnetic high strength stainless steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance, corrosion resistance...
Journal Articles
Alloy Digest (1968) 17 (3): SS-206.
Published: 01 March 1968
... URANUS-65 is a low-carbon, chromium-nickel heat and corrosion resistant austenitic stainless steel recommended for parts to resist high stresses and oxidation at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2000) 49 (9): SS-802.
Published: 01 September 2000
... Uranus 45N+ (UR 45N+) is a modification of the 2205 or UNS S31803 composition to which molybdenum and nitrogen have been optimized to develop a pitting resistance equivalent nitrogen (PREN) number that is 36 or greater. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1191.
Published: 01 November 2014
... Uranus 31 is a super-austenitic steel with very high nickel, chromium, and molybdenum content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2009) 58 (1): SS-1028.
Published: 01 January 2009
... URANUS 76N contains high chromium, molybdenum, and nitrogen contents and has a pitting resistance equivalent number (PREN) ≥ 40. These factors explain why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore applications...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1198.
Published: 01 January 2015
... Uranus UR 2205Mo is a high chromium, molybdenum, and nitrogen alloy (PREN ≥ 35) that is very resistant to localized corrosion even in acidified oxidizing environments. The alloy has been used in the chemical industry. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (7): SS-1124.
Published: 01 July 2012
... Uranus 4565 is a high N super austenitic stainless steel with a Pitting Resistance Equivalent Number (PREN) >45. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2004) 53 (9): SS-907.
Published: 01 September 2004
... The high chromium, molybdenum, and nitrogen contents of alloy Uranus B25 (also referred to as UR B25) and its pitting resistance equivalent number (PREN) of >=42 explain why the grade is very resistant to localized corrosion even in acidified oxidizing environments. The alloy has also been used...
Journal Articles
Alloy Digest (1999) 48 (8): SS-758.
Published: 01 August 1999
... Steel August 1999 URANUS 45NMo Temperature Young s modulus Shear modulus °C °F GPa 106 psi GPa 106 psi 20 68 200 29 75 10.9 100 212 190 28 73 10.5 200 392 180 27 70 10.1 300 572 170 26 67 9.7 See also Table 2. Table 1 Thermal and Electrical Properties Resistivity Thermal conductivity Specific heat...
Journal Articles
Alloy Digest (1996) 45 (9): SS-653.
Published: 01 September 1996
... Uranus 45N (UR 45N) is a nitrogen alloyed (>0.15%) austenitic-ferritic stainless steel (2205 type) with improved structural stability and high general, localized, and stress-corrosion resistance properties. The Pitting Resistance Equivalent Number (PREN) is >33. This datasheet provides...
Journal Articles
Alloy Digest (2015) 64 (3): SS-1204.
Published: 01 March 2015
... Uranus UR 2202 is considered a lean duplex austenitic/ferritic stainless steel designed to match the corrosion resistance of AISI Type 304L. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture...
Journal Articles
Alloy Digest (2006) 55 (11): SS-981.
Published: 01 November 2006
... CLI-SAF 2507 is a superaustenitic/ferritic duplex stainless steel with a pitting resistance equivalent number (PREN) greater than 40. This grade was formerly called Uranus 47N+ and is an overalloyed replacement variant of UR 47N (See Alloy Digest SS-564, March 1994). This datasheet provides...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-602.
Published: 01 February 2003
... 2.4697 (G-NiCr20Mo15) (cast) Proprietary Hastelloy alloy C22 (Haynes) Proprietary Nicrofer 5621hMoW (Krupp VDM) Superaustenitics ASTM/UNS S32654, S31254, S34565 Proprietary 654SMO (Avesta Polarit) Proprietary Uranus B66 (Usinor Industeel) HAS 59 may be used for dissimilar joints between any combination...