Alloy Digest (1964) 13 (5): Ni-91.
Published: 01 May 1964
... Unitemp-HX is a nickel-base material recommended for high temperature applications. It has outstanding oxidation resistance at high temperatures under most operating conditions, and good high-temperature strength. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1990) 39 (10): Co-80.
Published: 01 October 1990
... UNITEMP I-Ix* LlNllEMp*m5 "F ms/in2 miI/side mg/inz mil/side mg/in2 miI/side -- -- -- 1600 0.05 9.7 0.07 13.5 0.09 iii 253 8-G i-2 34.8 15.5 0.25 11 272.0 54 8 0.37 1 83 2100 59.4 0:39 59.4 0.42 685.0 4.57 *UNITEMP HX: Ni-B~.5-23Cr/8-10Mo/l7-20Fe/0.5-2Xo UNlTEMPL605: Co-Base/l9-21Cr/9-11Ni/l4-16W/3Fe...