Alloy Digest (1967) 16 (9): SS-199.
Published: 01 September 1967
... UNITEMP-1430MV is a martensitic high-chromium, molybdenum heat and corrosion resisting steel used for highly stressed parts involving service temperatures up to 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...