Alloy Digest (1971) 20 (12): Fe-48.
Published: 01 December 1971
... UNITEMP N-155 is an iron-base austenitic alloy used over a wide temperature range from subzero to about 1800 or 1900 F. It has relatively good oxidation and corrosion resistance. It is used in such applications as turbine rotors, shafts and blades, afterburner parts, nozzles and combustion...